Welding MCQs — Set 7

10 practice questions on welding defects — what causes porosity, cracks, undercut and other weld faults, and how to spot them.

Q1. What causes porosity in a weld?

  • (a) Gas trapped in the molten weld metal as it solidifies
  • (b) Too much filler metal
  • (c) A very short arc length
  • (d) Welding too slowly

Answer: (a) Gas trapped in the molten weld metal as it solidifies — gas from damp electrodes, a dirty joint or lost shielding forms bubbles that stay in the weld as pores.

Q2. What is slag inclusion in a weld?

  • (a) Slag trapped inside the weld metal between passes
  • (b) Extra filler metal on the surface
  • (c) A crack at the end of the weld
  • (d) Rust on the outside of the joint

Answer: (a) Slag trapped inside the weld metal between passes — if slag is not cleaned off before the next pass, it gets buried in the weld and weakens it.

Q3. What is undercut in welding?

  • (a) A groove melted into the parent metal beside the weld toe
  • (b) A weld that is too wide
  • (c) Slag left on the surface
  • (d) A weld made from underneath

Answer: (a) A groove melted into the parent metal beside the weld toe — undercut is usually caused by too high a current or too fast travel, and it weakens the joint.

Q4. Which of these is a common cause of cracks in a weld?

  • (a) Hydrogen in the weld metal combined with rapid cooling and restraint
  • (b) Using a welding helmet
  • (c) Cleaning the joint before welding
  • (d) Welding at the correct current

Answer: (a) Hydrogen in the weld metal combined with rapid cooling and restraint — hydrogen from moisture, fast cooling and a rigid joint together cause cold cracking, especially in high-strength steels.

Q5. What is lack of fusion in a weld?

  • (a) The weld metal fails to fuse with the parent metal or with the previous pass
  • (b) The weld is too hot
  • (c) The electrode melts too fast
  • (d) The slag is not chipped off

Answer: (a) The weld metal fails to fuse with the parent metal or with the previous pass — too little heat, a wrong electrode angle or a dirty joint leaves an unfused gap that weakens the weld.

Q6. What is spatter in welding?

  • (a) Molten metal droplets thrown out of the weld pool onto the surrounding surface
  • (b) A type of shielding gas
  • (c) The slag layer on top of the bead
  • (d) A welding helmet shade

Answer: (a) Molten metal droplets thrown out of the weld pool onto the surrounding surface — spatter is increased by too high a current or too long an arc.

Q7. What causes burn-through when welding thin sheet?

  • (a) Too low a current
  • (b) Too high a current or too slow travel, melting a hole through the sheet
  • (c) A dirty welding helmet
  • (d) Too much shielding gas

Answer: (b) Too high a current or too slow travel, melting a hole through the sheet — thin metal needs low current and fast travel, or a process with fine control such as TIG.

Q8. What causes distortion of a welded fabrication?

  • (a) Uneven heating and contraction of the metal as it cools
  • (b) The weight of the slag
  • (c) The colour of the electrode coating
  • (d) The length of the earth cable

Answer: (a) Uneven heating and contraction of the metal as it cools — the hot weld zone expands, then shrinks as it cools, pulling the plates out of shape unless the work is clamped or the welding is balanced.

Q9. What is a crater crack?

  • (a) A crack that forms in the small crater left at the end of a weld run
  • (b) A crack in the electrode holder
  • (c) A crack in the shielding gas hose
  • (d) A crack in the welding cable

Answer: (a) A crack that forms in the small crater left at the end of a weld run — the crater cools and shrinks quickly, so it cracks unless the welder fills it by pausing or back-stepping at the end of the run.

Q10. What is overlap (cold lap) in a weld?

  • (a) Weld metal that flows over the parent metal surface without fusing to it
  • (b) Two weld runs crossing each other
  • (c) Slag covering the whole bead
  • (d) A weld made with two electrodes at once

Answer: (a) Weld metal that flows over the parent metal surface without fusing to it — overlap is caused by too low a current or a wrong electrode angle, and it leaves a weak, unfused edge.

Also read: GFCI Outlet Keeps Tripping | All MCQ Topics